WanBlend® CA3250
Property Name | Value | Unit |
---|---|---|
Physical State | Solid | -- |
Relative density (water = 1) | 1.10 - 1.25 | -- |
Appearance | Granule | -- |
Auto-Ignition Temperature | > 390 | °C |
Decomposition Temperature | >= 380 | -- |
Melting point/freezing point | > 100 | °C |
Flash Point | > 400 | °C |
Solubility in Water | Immiscible | -- |
Specification Name | Value | Unit | Test Method | Test Condition |
---|---|---|---|---|
Yield Strain at 1 mm/min | 4 | -- | -- | -- |
Strain at Break at 50 mm/min | 100 | -- | -- | -- |
Flexural Strength at 2 mm/min | 90 | MPa | ASTM D790 | -- |
Flexural Modulus at 2 mm/min | 2700 | MPa | -- | -- |
Izod Notched Impact Strength at 23 °C | 650 | KJ/m2 | ASTM D256 | -- |
Heat Distortion Temp. at 1.80 MPa; 4.0 mm | 83 | °C | ASTM D648 | -- |
Vicat Softening Temp. at 120 °C/h; 50 N | 103 | °C | ASTM D1525 | -- |
Flame Rating at 1.5 mm | V0 | -- | UL 94 | -- |
Flame Rating at 3 mm | -- | -- | -- | -- |
Volume Resistivity | 10^14 | Ω·m | IEC 60093 | -- |
Surface resistivity | 10^16 | Ω | -- | -- |
Drying Temperature | 80 | °C | -- | -- |
Drying Time | 4 - 6 | h | -- | -- |
Injection Temperature | 240 - 270 | °C | -- | -- |
Mold temperature | -- | °C | -- | -- |
Tensile Modulus at 1 mm/min | 2500 | MPa | -- | -- |
Yield Stress at 50 mm/min | -- | % | -- | -- |
Melt flow Index at 260 °C/5 Kg | 18 | g/10min | ASTM D1238 | -- |
Mold Shrinkage | 0.5 - 0.7 | % | ASTM D955 | -- |
Water Absorption at 23°C, 24h | 0.2 | % | ASTM D570 | -- |
Density | 1.18 | g/cm3 | ASTM D792 | -- |
Stress at Break at 50 mm/min | 60 | MPa | ASTM D638 | -- |