Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity

Product Details
Customization: Available
Feature: Oxidative Degradable
CAS No.: 25037-45-0
Still deciding? Get samples of US$ 3/kg
Request Sample
Gold Member Since 2024

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Importers and Exporters
The supplier has import and export rights
High Repeat Buyers Choice
More than 50% of buyers repeatedly choose the supplier
Experienced Team
The supplier has 7 foreign trading staff(s) and 7 staff(s) with over 6 years of overseas trading experience
In-stock Capacity
The supplier has In-stock capacity
to see all verified strength labels (11)
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
  • Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
Find Similar Products
  • Overview
  • Product Description
  • Product Parameters
  • Applications
  • Company Profile
  • Packaging & Shipping
  • FAQ
Overview

Basic Info.

Model NO.
A1107
Material
Polycarbonates/PC
Usage
General Plastics, Engineering Plastics, Specialty Plastics
Plastic Properties After Heated
Thermoplastic Plastics
Plastic Forming Method
Injection
Color
Transparent Color
Application
High Flow Injection Molding Parts
Transport Package
25kg/Bag, 1000kg/Pallet
Specification
PC RESIN
Trademark
CLARNATE
Origin
Yantai
HS Code
3904220000
Production Capacity
5000

Product Description

 
Product Description

Clarnate® A1107

  • Features: Medium viscosity, Easy release, UV stabilized
  • Uses: General purpose
  • Appearance: Clear/ transparent
  • Forms: Pellets
  • Processing Method: Injection molding
Product Parameters

Properties

Property Name Value Unit
Appearance Granule --
Physical State Solid --
Relative density (water = 1) 1.18-1.20 --
Auto-Ignition Temperature >550 °C
Decomposition Temperature >380 --
Melting point/freezing point >240 °C
Flash Point >522 °C
Molecular Weight 516.58 g/mol
Solubility in Water Immiscible --

Specifications

 
 
Specification Name Value Unit Test Method Test Condition
Melt Flow Index at 300°C/1.2 Kg 10 g/10min ASTM D1238 --
Mold Shrinkage 0.5 - 0.7 % ASTM D955 --
Water Absorption at 23°C, 24h 0.2 % ASTM D570 --
Density 1.2 g/cm3 ASTM D792 --
Stress at Break at 50 mm/min 70 MPa ASTM D638 --
Tensile Modulus at 1 mm/min 2300 MPa -- --
Yield Stress at 50 mm/min 65 MPa -- --
Yield Strain at 50 mm/min 6 % -- --
Strain at Break at 50 mm/min 120 % -- --
Flexural Strength at 2 mm/min 98 MPa ASTM D790 --
Flexural Modulus at 2 mm/min -- MPa -- --
Izod Notched Impact Strength at 23 °C 780 J/m ASTM D256 --
Heat Distortion Temp. at 1.82 MPa; 3.2 mm 128 °C ASTM D648 --
Vicat Softening Temp. at 120 °C/h; 50 N 149 °C ASTM D1525 --
Haze at 3 mm < 0.8 % ASTM D1003 --
Light Transmittance at 3 mm 89 % -- --
Refractive Index 1.586 -- ASTM D542 --
Flame Rating at 3 mm HB -- UL 94 --
Flame Rating at 1.5mm V2 -- -- --
Relative Permittivity at 100 Hz 3.1 -- IEC 60250 --
Relative Permittivity at 1 MHz 3 -- -- --
Dissipation Factor at 100 Hz 5 10^-4 -- --
Dissipation Factor at 1 MHz 90 10^-4 -- --
Volume Resistivity 10^14 Ω·m IEC 60093 --
Surface resistivity 10^16 Ω -- --
Electric Strength at 1 mm 34 kV/mm IEC 60243-1 --
Comparative Tracking Index at Solution A 250 V IEC 60112 --
Drying Temperature -- °C -- --
Drying Time -- h -- --
Injection Temperature 280 - 310 °C -- --
Mold temperature 80 °C -- --
Injection Speed 50 mm/s -- --
 
 
 

 

Applications

Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity

Company Profile

Hoskimi Technology (Shanghai) Co., Ltd. Was established in 2010 and is located in Shanghai Hongqiao West Business District. It provides customers with timely technical service support, diversified multi-brand material supply, and optimal material selection suggestions and combinations. It has modern warehousing services and is committed to providing customers with the best cost-effective solutions and stable & reliable supply resources.
Plowing in the automotive industry for 14 years, has a wealth of experience in the automotive industry development and after-sales service, with Mercedes-Benz, BMW, Tesla, SAIC and other major automotive OEMs and Tier 1 Glammer, Xinquan, Changzhou Interior and other close cooperation, in the project there are many successful cases, such as SAIC RX5, SAIC MG SUV, SAIC Audi A7, Lixiang L6, Mercedes-Benz C. Class, SAIC Motor General Motors and etc.
Packaging & Shipping
Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
Wholesale Price Wanhua Clarnate A1107 Polycarbonate PC Polycarbonate Resin Granules with Medium Viscosity
 
FAQ

Q: Where is your company based?
A:Our company located in Room 501, 5/F, Xin'ao Business Building, No. 720 Huajiang Road, Jiading District, Shanghai, China.

Q:What can you buy from us?
A: PC, PC/ABS, Polymethyl methacrylate, ABS, PA, POM, TPE, TPV and Etc.

Q:Can we get your samples?
A:Yes! Samples can be arranged for those available products. The Delivery Fee will be on buyer's account.

Q:What are your terms of payment?
A:T/T, L/C,. Option A:30% pay in advance, 70% before shipping

Q: What is your packing?
A:Basically our packing is in 25/KG bags.

Q:Where is the loading port?
A:Usually Shanghai.

Q:What is the normal lead time?
A:  We will send goods to departure port within 5-10 workdays after we receive your payment.

Q:If any quality problem, how can you settle it for us?
A: When discharging the container, you need to inspect all the goods. If any breakage or defect products were found, you MUST take the pictures from the original carton. All the claims must be presented within 7 working days after discharging the container. This date is subject the arrival time of container. We will advise you to certify the claim by third party, or we can accept the claim from the samples or pictures you present, discharging of the container is not included. Finally we will completely compensate all your loss.

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier